777-11 Laser repair cladding of K418 Ni-base superalloy by CoCrNiW powder. Chen C, Cao O, Zhang M. ADVANCED MATER. RES., 2011, 291/294(2), 1417-1420.
|
778-11 Study of laser cladding novel Co-9Al-7.5W superalloy on 304 stainless steel. Xu Y, Zhao W, Xia T. ADVANCED MATER. RES., 2011, 291/294(2). 872-877.
|
779-11 Effect of nitrogen on microstructure and properties of a cast cobalt-base superalloy. Yuan C, Guo J, Zhou L. ADVANCED MATER. RES., 2011, 278, 472-478.
|
780-11 Morphology change of gamma' precipitates in gamma/gamma' two-phase microstructure in Co-based superalloys by higher-order alloying. Tanaka K, Ooshima M, Okamoto N. MATER. RES. SOC. SYMPOSIUM PROCEEDINGS, 2011, 1295, 423-428.
|
781-11 Effects of high temperature deformation and thermal exposure on micrsotructure and mechanical properties of Co-based superalloy. Lee H, Yoo K, Song K. ADVANCED MATER. RES., 2011, 275(121-124.
|
782-11 Characterising and reducing seizure wear of inconel and incoloy superalloys in a sliding contact. Houghton A, Lewis R, Olofsson U. WEAR, 2011, 271(9-10), 1671-1680.
|
783-11 Activation energy of oxidation of novel Co-Al-W superalloys at high temperatures. Yangtao X, Tiangdong X, Wenjun Z. RARE METAL MATERS. & ENGINEERING, 2011, 40(4), 701-704.
|
784-11 Static recrystallisation kinetics of Haynes230 superalloy. Peng C, Chang H, Hu R. J. AERONAUTICAL MATERS., 2011, 31(2), 8-12.
|
785-11 Effect of B and Cr on the high temperature oxidation behaviour of novel g/gprime-strengthened Co-base superalloys. Klein L, Shen Y, Killian M. CORROSION SCI., 2011, 53(9), 2713-2720.
|
786-11 High temperature SO2-gas corrosion of Ni-Cr-Co base superalloy between 800 and 1000°C. Bak S, Lee D. DIFFUSION & DEFECT DATA A, 2011, 312/315(1), 451-454.
|
787-11 The impact of cermaic shell strength on hot tearing during investment casting in a cobalt-base superalloy. Norouzi S, Farhangi H. AIP CONF. PROCEEDINGS, 2010, 1315(1), 662-670.
|
July 2011 |
530-11 An assessment of cumulative axial and torsional fatigue in a cobalt-base superalloy. Kalluri S, Bonacuse P. ASTM SPECIAL TECHNICAL PUBLICATION, 2011, 1526, 421-440.
|
531-11 Strain-induced phase transformation in a cobalt-based superalloy during different loading modes. Benson M, Liaw P, Choo H. MATERS SCI. & ENGINEERING A, 2011, 528(18), 6051-6058.
|
532-11 Effects of heat treatments on the serrated flow in a Ni-Co-Cr base superalloy. Cui C, Jin T, Sun Z. J. MATERS SCI., 2011, 46(16), 5546-5552.
|
533-11 Enhanced mechanical properties in a new Ni-Co base superalloy by controlling microstructures. Cui C, Gu Y, Yuan Y. MATERS. SCI. & ENGINEERING A, 2011, 528(16-17), 5465-5469.
|
534-11 The impact of ceramic shell strength on hot tearing during investment casting in a cbalt-base superalloy. Norouzi S, Farhangi H. AIP CONF. PROCEEDINGS, 2010, 1315, Part 1, 662-670.
|
535-11 Effect of processing parameters on hot compressive deformation behaviour of a new Ni-Cr-Co based P/M superalloy. Wu K, Liu G, Hu B. MATERS. SCI. & ENGINEERING A, 2011, 528(13-14), 4620-4629.
|
536-11 High temperature oxidation of g/gprime-strengthened Co-base superalloys. Klein L, Bauer A, Neumeier S. CORROSION SCI., 2011, 53(5), 2027-2034.
|
537-11 Oxidation-resistant properties of a Co-Cr-Ni-W superalloy. Xiao X, Liu Y. J. FUNCTIONAL MATERS., 2010, 41(Supp/3), 476-479.
|
538-11 Factors contributing to the strength of a polycrystalline nickel-cobalt base superalloy. Osada T, Nagashima N, Gu Y. SCRIPTA MATERIALIA, 2011, 64(9), 892-895.
|
539-11 Hot corrosion behaviour of a cobalt-base superalloy K40S with and without NiCrAlYSi coating. Zhang K, Liu M, Liu S. CORROSION SCI., 2011, 53(5), 1990-1998.
|
April 2011 |
310-11 Hot compressive deformation behaviour of a new hot isostatically pressed Ni-Cr-Co based powder metallurgy superalloy. Wu K, Liu G, Hu B. MATERS. & DESIGN, 2011, 53(1-4), 1872-1879.
|
311-11 Phase-transformation and subgrain-deformation characteristics in a cobalt-based superalloy. Benson M, Reetz B, Liaw P. MATERS SCI. & ENGINEERING A, 2011, 528(4-5), 1987-1993.
|
312-11 Dynamic strain aging in a new Ni-Co base superalloy. Cui C, Gu Y, Yuan Y. SCRIPTA MATERIALIA, 2011, 64(6), 502-505.
|
January 2011 |
138-11 Effect of several alloying elements on electrochemical corrosion behaviour of a novel superalloy Co-Al-W superalloy. Xu Y, Xia T, Yan J. CORROSION SCI. & PROTECTION TEHCNOL., 2010, 22(5), 371-376.
|
|
|