October 2008

Hard Materials

623-08
Gelcasting of WC-8wt%Co tungsten cemented carbide. Li Y, Guo Z. INTNL J. REFRACTORY METALS & HARD MATERIALS, 2008, 26(5), 472-477.
624-08
Effects of electrical discharge energy on machining performance and bending strength of cemented tungsten carbides. J. MATER. PROCESSING TECHNOL., 2008, 206(1-3), 491-499.
625-08
Analytical modelling to calculate the hardness of ultra-fine WC-Co cemented carbides. Cha S, Lee K, Ryu H. MATER. SCI. & ENGINEERING A, 2008, 489(1-2), 234-244.
626-08
Numerical simulation of kinetics of the cobalt gradient change in WC-Co during liquid phase sintering. Fan P, Fang Z, Prichard P. MATER. SCI. & TECHNOL., 2007, 3, 1618-1627.
627-08
Al-enhanced nucleation and adhesion of diamond films on WC-Co substrates. Li Y, Tang Y, Yang. INTNL J. REFRACTORY METALS & HARD MATERIALS. 2008, 26(5), 465-471.
628-08
Temperature distribution and neck formation of WC-Co combined particles during spark plasma sintering. Liu X, Song, Zhang J. MATER. SCI. & ENGINEERING A, 2008, 488(1-2), 1-7.
629-08
Study on the local damage mechanisms in WC-Co hard metals during scratch testing. Ndlovu S, Durst K, Hoeppel H. 2007, 1049, 75-84.
630-08
Change in relative density of WC-Co cemented carbides in spark plasma sintering process. Sun L, Lin C, Jia C. REARE METALS, 2008, 27(1), 74-77.
631-08
Influence of notch radius and R-curve behaviour on the fracture toughness evaluation of WC-Co cemented carbides. Torres Y, Bermejo R, Llanes L. ENGINEERING FRACTURE MECHANICS, 2008, 75(15), 4422-4430.
632-08
ICP-MS, SKPFM, XPS and microcapillary investigation of the local corrosion mechanisms of WC-Co hardmetal. Hochstrasser-Kurz S, Reiss D, Suter T. J. ELECTROCHEMICAL SOC., 2008, 155(8), C415-C426.

July 2008

452-08
On the abrasion of ultrafine WC-Co hardmetals by small SiC abrasive. Krakhmalev P. TRIBOLOGY LETTERS, 2008, 30(1), 35-39.
453-08
Properties and microstructure of VC/Cr3C2-doped WC/Co cemented carbides. Lei Y, Sun J, Du X. RARE METALS, 2007, 26(6), 584-590.
454-08
A streamline life cycle assessment on the fabrication of WC-Co cermets. Xiong Y, Lau K, Zhou X. J. CLEANER PRODUCTION, 2008, 16(10), 1118-1126.
455-08
A study of diamond film deposition on WC-Co inserts for graphite machining: Effectiveness of SiC interlayers prepared by HFCVD. Cabral G, Gäbler J, Lindner J. DIAMOND & RELATED MATERIALS, 2008, 17(6), 1008-1014.
456-08
A novel route to prepare ultrafine-grained WC-Co cemented carbides. Liu W, Song X, Zhang J. J. ALLOYS & COMPOUNDS, 2008, 458(1-2), 366-371.
457-08
Parameters optimisation in the planetary ball milling of nanostructured tungsten carbide/cobalt powder. Zhang F, Zhu M, Wang. INTNL J. REFRACTORY METALS AND HARD MATERIALS. 2008, 26(4), 329-333.
458-08
Effect of size and location of spherical pores on transverse rupture strength of WC-Co cemented carbides. Cha S, Lee K, Ryu H. MATERIALS SCI. & ENGINEERING A, 2008, 486(1-2), 404-408.
459-08
Some analytical consequences of experimental data on properties of WC-Co hardmetals. Golovchan V. INTNL J. REFRACTORY METALS & HARD MATERIALS, 2008, 26(4), 301-305.
460-08
Morphology of WC grains in WC-Co alloys. Lay S, Allibert C, Christensen M. MATERIALS SCI. & ENGINEERING A, 2008, 486(1-2), 253-261.
461-08
Crack propagation characteristic and toughness of functionally graded WC-Co cemented carbide. Zhang L, Wang Y, Yu X. INTNL J. REFRACTORY METALS & HARD MATERIALS, 2008, 26(4), 295-300.

April 2008

301-08
Structure and properties of WC-Co alloys in solid-phase sintering. II. Mechanical properties of
302-08
Characterisation of nanostructured WC-Co deposited by cold spraying. Li C, Yang G, Gao P. J. THERMAL SPRAY TECHNOL., 2007, 16(5-6), 1011-1020.
303-08
Special WC/Co orientation relationship at basal facets of WC grains in WC-Co alloys. Bounhoure V, Lay S, Loubradou M. J. MATER SCI, 2008, 43(3), 892-899.
304-08
Effects of scale combination and contact condition of raw powders on SPS sintered near-nanocrystalline WC-Co alloy. Zhao S, Song X, Zhang J. MATERIALS SCI. & ENGINEERING A, 2008, 473(1-2), 323-329.
305-08
Structure and propertyies of WC-Co alloys in solid-phase sintering. I. Geometrical evolution. Laptev A, POWDER MET. & METAL CERAMICS, 2007, 46(9-10), 415-422.

 