January 2006 |
Hard Materials |
138-06 A comparative study on cutting performance of TiN-coated tungsten carbide cutting tool with a cobalt interlayer. Hee Kwon D, Chang Kang M, Suk Kim J.
|
139-06 Development in the model-industry: Micro-machining of hard metal (WC-10% Co) by Nd@YAG laser. Yeh L, Heelrung D, Gillner A.
|
140-06 Effect of WC/TiC grain size ratio on microstructure and mechanical properties of WC-TiC-Co cemented carbides. Lee K, Cha S, Kim B.
|
141-06 Effects of microstructures and machining conditions on surface roughness of WC-Co cemented carbides machined by focused ion beam. Hosokawa H, Shimojima K, Mabuchi M.
|
142-06 An experimental study of the sintering of nanocrystalline WC-Co powders. Fang Z, Maheshwari P, Wang X.
|
143-06 Extrapolating hardness-structure property maps in WC/Co hardmetals. Roebuck B.
|
144-06 Growth behaviour of rounded (Ti,W)C and faceted WC grains in a Co matrix during liquid phase sintering. Yoon B, Lee B, Kang S.
|
145-06 Liquid phase sintering of functionality graded WC-Co composites. Eso O, Fang Z, Griffo A.
|
146-06 Mechanical properties of WC/Co cemented carbide with larger WC grain size. Okamoto S, Nakazono Y, Otsuka K.
|
147-06 Nucleation rate of diamond films on WC-Co alloys. Liu S.
|
148-06 Sintering shrinkage of WC-Co materials with different compositions. Petersson A, Gren J.
|
149-06 The temperature ranges for maximum effectiveness of grain growth inhibitors in WC-Co alloys. Morton C, Wills D, Stjernberg K.
|
150-06 Thermodynamic analysis of the reduction processes during the production of cemented carbides. Bondarenko V, Epik I.
|
October 2005 |
0703-05 "Application of a wax-based binder in PIM of WC-TiC-Co cemented carbides. Qu X, Gao J, Qin M."
|
0704-05 "Cobalt-based alloy PTA hardfacing on different substrate steels. Yaedu A, Oliveira A."
|
0705-05 "Density, structure and properties of ultrafine WC-(20-50)%Co hardmetals obtained by pressing in solid state. Tolochyn O, Laptev A, Kovyliaev V."
|
0706-05 "Determination of the conditions for surface grinding of cemented carbides by applying a new concept of current limited cutting ability of a wheel. Matyykha P, Strelkov V, Poltavets V."
|
0707-05 "Diamond deposition on WC/Co alloy with a molybdenum intermediate layer. Liu S, Yu Z, Yi D."
|
0708-05 "Effect of corrosion environment on the fatigue behaviour of WC-Co hard alloy teeth of drill bits. Vasyliv B, Ivasyshyn A, Ostash O."
|
0709-05 "Enhanced densification of liquid-phase-sintered WC-Co by use of coarse WC powder: Experimental support for the pore-filling theory. Kim Y, Jung S, Kang S."
|
0710-05 "An experimental study of the sintering of nanocrystalline WC-Co powders. Fang Z, Maheshwari P, Wang X."
|
0711-05 "Influence of NbC-addition on mechanical properties of WC-Co. Acchar W, de Macedo H."
|
0712-05 "Laser sintering (SLA) of hard metal powders for abrasion resistant coatings. Maeda K, Childs T."
|
0713-05 "Liquid phase sintering of functionally graded WC-Co composites. Eso O, Fang Z, Griffo A."
|
0714-05 "Mechanisms of fatigue crack growth in WC-Co cemented carbides. Boo M, Park C."
|