October 2007 |
Alloys |
791-07 Heterogeneous and homogeneous nanoscale precipitation in dilute Cu-Co alloys. Rocha A, Solorzano I, Vander Sande J.
|
792-07 Effect of electrospark dispersion on the martensitic transformation in Co-Fe-Ni-Ti-(Cu) alloys. Gun'ko L, Zalutskii V, Perekos A.
|
793-07 In situ observation of magnetic domain structure in Co50Ni20FeGa29 alloy under the applied magnetic field. Wang H, Dai X, Wang Y.
|
794-07 Effect of Co content on the catalytic activity of CoSiBEA zeolite in the selective catalytic reduction of NO with ethanol: Nature of the cobalt species. Janas J, Machej T, Gurgul J.
|
795-07 TEM characterisation of twinning in Co39Ni33Al28 Alloy. Wang H, Wang K, Liu Z.
|
796-07 Structural and magnetic transitions in Fe-, Co- and Al-substituted Ni-Mn-Ga Ferromagnetic shape memory alloys. Mathur R, Singh R, Chandrasekaran V.
|
July 2007 |
545-07 A potential Co36Fe36Si4B20Nb4 nanocrystalline alloy for high temperature soft magnetic applications. Panda A, Mohanta O, Kumar A.
|
546-07 Cobalt alloys and composites. Freels M, Liaw P, Jiang L.
|
547-07 Hydrogenation properties and crystal structure of the single BCC (Ti0.355V0.645)100-xMx alloys with M = Mn, Fe, Co, Ni (x = 7, 14 and 21). Challet S, Latroche M, Heurtaux F.
|
548-07 Influence of initial phase composition on glass-forming ability of Co-based alloys. Chikina E, Dyakonova N, Molokanov V.
|
549-07 Microstructure and corrosion resistance of medical cobalt-based alloys. Shengfeng S, Jun L, Bing Z.
|
550-07 Tensile property of cold-rolled foils of Ni-based and Co-based L12 intermetallic alloys. Kaneno Y, Takasugi T, Myoki T.
|
551-07 Thermodynamic assessments of the Cu-Mn-X (X: Fe, Co) systems. Wang C, Liu X, Ohnuma I.
|
April 2007 |
321-07 Controllable synthesis and magnetic properties of Fe-Co alloy nanoparticles attached on carbon nanotubes. Wu H, Yuan P, Xu H.
|
322-07 Copper line resistance behaviour in Pd-activated Co alloy capping process. Wang X, Owatari A, Ishibashi T.
|
323-07 Martensitic and magnetic transformation of Co41Ni32Al24Sb3 and Co41Ni32Al27 alloys. Xu G, Yin Z, Luo F.
|
324-07 Microstructural characteristics and vibration fracture properties of Sn-Ag-Cu-TM (TM = Co, Ni and Zn) alloys. Song J, Huang C, Chuang H.
|
325-07 On the ternary Laves phases {Sc,Ti}2M3Si (M = Cr, Mn, Fe, Co, Ni) with MgZn2-type. Yan X, chen X, Grytsiv A.
|
326-07 Effect of growth rate on directionally solidified microstructure of Cu-7.9% Co Peritectic alloy. Binglun J, Shuangming L, Lin L.
|
327-07 Microstructural characterisation of as-cast Co-B alloys. Faria M, Leonardi T, Coelho G.
|
328-07 Studies of electroless Ni-Co-P ternary alloy on glass fibres. Huang Y, Shi K, Liao Z.
|
329-07 Initial stages of the electrocrystallisation of Co-Cu alloys on GCE from the Co rich electrolytes. Gu M.
|
January 2007 |
001-07 Amorphisation and crystallisation processes of the ball-milled Al-Y-Fe-TM alloys ( TM = Ni, Co, Cu and Fe). Wilson T, Choo H, Porter W.
|
002-07 Corrosion-stable nickel- and cobalt-based alloys for dental applications. Rahm E, Kunzmann D, Doring H.
|